Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 11.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
11.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem 1100EF PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 11.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
11.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem 1100EF PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 11.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
11.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem 1100EF PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||
Melt Flow | 11.8 g/10 min @Load 5.00 kg, Temperature 265 °C |
11.8 g/10 min @Load 11.0 lb, Temperature 509 °F |
Procedure A; ASTM D1238 |
Diamond Polymers ABS TX-541 Description: Super High Heat ABSInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 11.8 g/10 min @Load 3.80 kg, Temperature 230 °C |
11.8 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers DIAMALOY 750 ABS/PC Alloy, Non-Halogen, Flame Retardant Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |