Polymer Property : Melt Flow = 13 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 9.0 - 13 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 - 13 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 2062U (62111) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 9.0 - 13 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 - 13 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 4052U (52411) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 9.0 - 13 g/10 min

@Load 3.80 kg,
Temperature 230 °C
9.0 - 13 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ABS 3501 SHF
Description: Super High FlowInformation provided by Diamond Polymers, Inc.
Melt Flow 7.0 - 13 g/10 min

@Load 3.80 kg,
Temperature 230 °C
7.0 - 13 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Solvay Specialty Polymers Solef® 9009 Polyvinylidene Fluoride (PVDF)  (discontinued **)
Solef® 9009 PVDF homopolymer has low/medium viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers.