Physical Properties Metric English Comments
Melt Flow 13.5 g/10 min

@Load 5.00 kg,
Temperature 210 °C
13.5 g/10 min

@Load 11.0 lb,
Temperature 410 °F
ASTM D1238
SABIC Innovative Plastics NORYL WCP781 PPE-TPE
Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto..
Melt Flow 13.5 g/10 min

@Load 5.00 kg,
Temperature 210 °C
13.5 g/10 min

@Load 11.0 lb,
Temperature 410 °F
ASTM D1238
SABIC Innovative Plastics NORYL WCP781 PPE-TPE (Asia Pacific)
Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto..
Melt Flow 13.5 g/10 min

@Load 5.00 kg,
Temperature 210 °C
13.5 g/10 min

@Load 11.0 lb,
Temperature 410 °F
ASTM D1238
SABIC Innovative Plastics NORYL WCP781 PPE-TPE (Europe-Africa-Middle East)
Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto..