Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 13.7 g/10 min @Load 6.60 kg, Temperature 337 °C |
13.7 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |