Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 19.6 g/10 min @Load 5.00 kg, Temperature 280 °C |
19.6 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D 1238 |
SABIC Innovative Plastics Noryl PX0346 PPE+PS This data was supplied by SABIC-IP for the Americas region. |