Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.1 - 2.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.1 - 2.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
±10% |
Kazanorgsintez PE2NT 18-11 Linear Low Density Polyethylene Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez |
|||
Melt Flow | 2.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal (POM)
(Unverified Data**) Toughened High Viscosity Acetal Homopolymer Delrin 100T NC010 is a toughened high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |
|||
Melt Flow | 2.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Delrin® 127UVE NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 127UVE NC010 (formerly DE20555) is a high viscosity acetal homopolymer with UV stabilizers with very low VOC emissions .. |
|||
Melt Flow | 2.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Delrin® 127UVE RD402 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 127UVE RD402 (formerly DE20555) is a high viscosity acetal homopolymer with UV stabilizers pigmented red with very low .. |
|||
Melt Flow | 2.1 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.1 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers ABS 3501ELG High Impact, Low Gloss Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 2.1 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.1 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS 9301 Description: Extrusion Grade, Low GlossInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.1 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.1 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ASA TW-15H Description: ASA Weatherable Polymer, Injection Molding Grade, High Heat Resistance, High IzodInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.1 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.1 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ASA TWP 155 Description: Transparent Weatherable PolymerInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Delrin® 100PE NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100PE NC010 (formerly DE20573) is a high viscosity acetal homopolymer an enhanced version of Delrin 100P with very low VOC emissions... |
|||
Melt Flow | 2.1 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
DuPont Performance Polymers Hytrel® HTR8139BK Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR8139BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nomin.. |
|||
Melt Flow | 2.1 g/10 min @Load 5.00 kg, Temperature 190 °C |
2.1 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Borealis Borstar® FB4370 Medium Density Polyethylene Borstar® FB4370 is a linear medium density polyethylene grade combining excellent extrusion properties with high film stiffness. Applications: Borstar® FB4370 has been developed especially for ap.. |