Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 18 - 24 g/10 min @Load 21.6 kg, Temperature 190 °C |
18 - 24 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 4222M (224F7) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 18 - 24 g/10 min @Load 5.00 kg, Temperature 230 °C |
18 - 24 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 41308 Polyvinylidene Fluoride (PVDF) Solef® 41308/0001 PVDF is specifically developed for coextrusion.Additional Properties: Crystallization Heat - ASTM D3418 51.6 J/g; Heat of Fusion - ASTM D3418 52.7 J/gInformation provided by Sol.. |
|||
Melt Flow | 18 - 24 g/10 min @Load 5.00 kg, Temperature 230 °C |
18 - 24 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 42308 Polyvinylidene Fluoride (PVDF) Solef® 42308 PVDF is specifically developed for coextrusion.Additional Properties: Crystallization Heat - ASTM D3418 51.6 J/g; Heat of Fusion - ASTM D3418 52.7 J/gInformation provided by Solvay S.. |
|||
Melt Flow | 18 - 24 g/10 min @Load 5.00 kg, Temperature 230 °C |
18 - 24 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 41308 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 41308/0001 PVDF is specifically developed for coextrusion.Information provided by Solvay Specialty Polymers. |