Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 29.8 g/10 min @Load 21.6 kg, Temperature 190 °C |
29.8 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Diamond Polymers NPP50-1111 TF20 20% Talc Filled White High Density Polyethylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |