Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.1 g/10 min @Load 1.00 kg, Temperature 235 °C |
3.1 g/10 min @Load 2.20 lb, Temperature 455 °F |
Procedure A Condition Q; ASTM D1238 |
Network Polymers Softflex® 7210 Black Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 3.1 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.1 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM Test |
Styrolution Terluran® GP-35 ABS Terluran GP-35 is a very high flow grade of ABS for injection molding with good resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF an.. |
|||
Melt Flow | 3.1 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.1 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Denka TH-11 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |