Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.9 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.9 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Denka TH-21 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Melt Flow | 3.9 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.9 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Denka TP-803 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Melt Flow | 3.9 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.9 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS/PC 9901 Description: Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 3.9 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.9 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers ABSPC 9901 ELG ABS/PC Injection Molding Grade, Very High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 3.9 g/10 min @Load 10.0 kg, Temperature 220 °C |
3.9 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Diamond Polymers ASA S-150E-1115 ASA Weatherable Polymers Extrusion Grade, Medium Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 3.9 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.9 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers DIAMALOY 750 ABS/PC Alloy, Non-Halogen, Flame Retardant Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 3.9 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.9 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ASA TWP 502 Description: Transparent Weatherable PolymerInformation provided by Diamond Polymers, Inc. |