Physical Properties Metric English Comments
Melt Flow 4.7 g/10 min

@Load 2.16 kg,
Temperature 240 °C
4.7 g/10 min

@Load 4.76 lb,
Temperature 464 °F
ISO 1133
DSM Arnitel® EM630 Polyether Ester Elastomer (European Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..