Polymer Property : Melt Flow = 44 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 44 g/10 min

@Load 1.20 kg,
Temperature 300 °C
44 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® OQ1060 PC Copolymer
Optical quality, high flow, high purity Polycarbonate copolymer resin with reduced oxygen transmission for advanced DVD applications such as Limited Play DVD.This data was supplied by SABIC-IP for t..
Melt Flow 44 g/10 min

@Load 1.20 kg,
Temperature 300 °C
44 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance.
Melt Flow 44 g/10 min

@Load 1.20 kg,
Temperature 300 °C
44 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER (Asia Pacific)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance.
Melt Flow 44 g/10 min

@Load 1.20 kg,
Temperature 300 °C
44 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER (Europe-Africa-Middle East)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance.
Melt Flow 44 g/10 min

@Load 21.6 kg,
Temperature 190 °C
44 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Borealis BL2631 High Density Polyethylene
BL2631 is a high density polyethylene homopolymer intended for blow molding of products requiring high toughness and stiffness. Applications: fresh milk bottles, and juice bottles.Information provi..