Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 49 g/10 min @Load 5.00 kg, Temperature 230 °C |
49 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Borealis ME266U Polypropylene Compound, Mineral Filled ME266U is a 20% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and gives a good surface quality. .. |
|||
Melt Flow | 49 g/10 min @Load 2.16 kg, Temperature 260 °C |
49 g/10 min @Load 4.76 lb, Temperature 500 °F |
ISO 1133 |
Polyplastics TOPAS® 5013 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade) This grade is characterized by its high flowability and superior optical properties. It is suitable for optical components such as lenses and light guide panels where high molded precision is indisp.. |
|||
Melt Flow | 49 g/10 min @Load 1.00 kg, Temperature 190 °C |
49 g/10 min @Load 2.20 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont™ Fusabond® P613 Polymer Modifier DuPont™ Fusabond® P613 is a anhydride modified polypropylene. FUSABOND P613 resin conforms with the Code of Federal Regulations, Title 21, Paragraph 175.105, covering the use of adhesive interlay.. |