Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.4 - 5.2 g/10 min @Load 5.00 kg, Temperature 190 °C |
2.4 - 5.2 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
BASF Ecovio® C2224 F Blend Biodegradable Polyester Description: Ecovio® F Blend C2224 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci.. |