Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 45 - 65 g/10 min @Load 5.00 kg, Temperature 200 °C |
45 - 65 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Versaflex™ OM 1245X-1 Thermoplastic Elastomer (TPE) The Versaflex™ OM 1245X-1 is designed for overmolding onto polycarbonate (PC), ABS, and PC/ABS susbstrates. - Excellent Bond to PC, ABS, PC/ABS - Rubbery Feel - Soft TouchColor concentrates with EV.. |