Physical Properties Metric English Comments
Melt Flow 7.4 g/10 min

@Load 2.16 kg,
Temperature 260 °C
7.4 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ISO 1133
Topas Advanced Polymers TOPAS® 9903D-10 Cyclic Olefin Copolymer (COC)
TOPAS® 9903D-10 is a very low glass transition temperature (Tg=33°C) film extrusion grade. It is designed to deliver high shrinkage at low temperatures in shrink packaging applications. It is a mo..