Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 70.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
70.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBB1232 Linear Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (450000 ppm) Features: Copolymer Uses: Compounding Forms: Pellets Processing Method: Compoundin.. |