Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 660 - 840 g/10 min @Load 21.6 kg, Temperature 190 °C |
660 - 840 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 4020W (20425) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 660 - 840 g/10 min @Load 21.6 kg, Temperature 190 °C |
660 - 840 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 4025W (25425) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |