Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Oxygen Transmission = 0.0140 cc-mm/m²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission 0.0140 cc-mm/m²-24hr-atm
0.0356 cc-mil/100 in²-24hr-atm
20°C- 65% RH; based on 20 µm layer
Noltex Soarnol® ET3803 Ethylene Vinyl Alcohol Copolymer
Medium ethylene content. Suitable for packaging a wet product in a wet environment. Preferred for use in forming webs for meat and cheese packaging. Ethylene content 38 mol%. Volatile matter 0.3%...
Oxygen Transmission 0.0140 cc-mm/m²-24hr-atm
0.0356 cc-mil/100 in²-24hr-atm
20°C- 65% RH; based on 20 µm layer
Noltex Soarnol® ET3808 Ethylene Vinyl Alcohol Copolymer
Ethylene content 38 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a..
Oxygen Transmission 0.0140 cc-mm/m²-24hr-atm
0.0356 cc-mil/100 in²-24hr-atm
20°C; 65% RH; Permeability increases significantly at higher moisture content.
EVALCA EVAL® LC-H101BD Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
38 mol % Ethylene.Data provided by EVALCA. Applications: Blown film. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of th..
Oxygen Transmission 0.0140 cc-mm/m²-24hr-atm
0.0356 cc-mil/100 in²-24hr-atm
20°C; 65% RH; Permeability increases significantly at higher moisture content.
EVALCA EVAL® K102 Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
38 mol % Ethylene.Data provided by EVALCA. Applications: Solid phase pressure forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produc..
Oxygen Transmission 0.0140 cc-mm/m²-24hr-atm
0.0356 cc-mil/100 in²-24hr-atm
Dow Saran® F-239 PVDC
SARAN® barrier resin F-239 is used for coating cellophane and polyester film. It is applied from a tetrahydrofuran/toluene solvent system, and gives coatings with excellent adhesion and transparenc..
Copyright © lookpolymers.com All Rights Reserved