Physical Properties Metric English Comments
Oxygen Transmission 0.0300 cc-mm/m²-24hr-atm
0.0762 cc-mil/100 in²-24hr-atm
20°C- 65% RH; based on 20 µm layer
Noltex Soarnol® A4412 Ethylene Vinyl Alcohol Copolymer
Ethylene content 44 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a..
Oxygen Transmission 0.0300 cc-mm/m²-24hr-atm
0.0762 cc-mil/100 in²-24hr-atm
20°C- 65% RH; based on 20 µm layer
Noltex Soarnol® AT4403 Ethylene Vinyl Alcohol Copolymer
High ethylene content, low melting point. Suitable for use in multilayer structures where ease of thermoforming is required. Ethylene content 44 mol%.The gas barrier property of Soarnol is about fo..
Oxygen Transmission 0.0300 cc-mm/m²-24hr-atm
0.0762 cc-mil/100 in²-24hr-atm
20°C; 65% RH; Permeability increases significantly at higher moisture content.
EVALCA EVAL® LC-E105A Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
44 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, melt phase forming, solid phase pressure forming, tubes, coex coating. EVOH is used in packaging applications because of its out..
Oxygen Transmission 0.0300 cc-mm/m²-24hr-atm
0.0762 cc-mil/100 in²-24hr-atm
20°C; 65% RH; Permeability increases significantly at higher moisture content.
EVALCA EVAL® LC-E151B Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
44 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming, solid phase pressure forming, blow molding, tubes EVOH is used in packaging applications because of its outstanding gas..
Oxygen Transmission 0.0300 cc-mm/m²-24hr-atm
0.0762 cc-mil/100 in²-24hr-atm
20°C; 65% RH; Permeability increases significantly at higher moisture content.
EVALCA EVAL® EF-E Ethylene Vinyl Alcohol Copolymer Film  (discontinued **)
44 mol % Ethylene. Non oriented type film; property values for 20 µm film.Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier pr..