Polymer Property : Oxygen Transmission = 0.0838 cc-mil/100 in²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission 0.0330 cc-mm/m²-24hr-atm
0.0838 cc-mil/100 in²-24hr-atm
Dow Saran® F-310 PVDC
SARAN® resin F-310 is a general purpose non crystalline copolymer offering moderate barrier. Its commercial applications include abrasion resistant binder for magnetic tapes, and barrier coating fo..