Physical Properties Metric English Comments
Oxygen Transmission 0.0433 cc-mm/m²-24hr-atm
0.110 cc-mil/100 in²-24hr-atm
blown film sample; ASTM D3985-81
Dow XU 32046.31 Barrier Polymer
Excellent oxygen and water vapor barrier Information provided by Dow