Polymer Property : Oxygen Transmission = 0.130 cc-mm/m²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission 0.130 cc-mm/m²-24hr-atm
0.330 cc-mil/100 in²-24hr-atm
Tested per ASTM D3985 at 22°C
DuPont Teijin Films Mylar® OB01 Polyester Packaging Film, 50 Gauge
Data provided by DuPont Packaging Polymers.Mylar® OB01 (formerly known as XM924) is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and a polyvinylidene chlor..