Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 0.300 - 0.900 cc-mm/m²-24hr-atm @Thickness 0.0600 mm |
0.762 - 2.29 cc-mil/100 in²-24hr-atm @Thickness 0.00236 in |
film; JIS Z7126 |
Kaneka PHBH Rigid Bio-based Polymer A copolymer produced of 3-hydroxybutyrate and 3-hydroxyhexanoate produced by fermentation of plant oils. It has excellent biodegradability (under anaerobic, aerobic, aquatic, and compost conditions.. |
|||
Oxygen Transmission | 0.300 - 0.900 cc-mm/m²-24hr-atm @Thickness 0.0600 mm |
0.762 - 2.29 cc-mil/100 in²-24hr-atm @Thickness 0.00236 in |
film; JIS Z7126 |
Kaneka PHBH Semi-Rigid Bio-based Polymer A copolymer produced of 3-hydroxybutyrate and 3-hydroxyhexanoate produced by fermentation of plant oils. It has excellent biodegradability (under anaerobic, aerobic, aquatic, and compost conditions.. |