Oxygen Transmission 0.470 cc-mm/m²-24hr-atm
1.19 cc-mil/100 in²-24hr-atm
40% RH, 23°C
DuPont Selar® PA 3426 Nylon Barrier Resin
Selar® PA 3426 is an amorphous nylon (polyamide) resin which exhibits superior transparency, good barrier properties to gases, water, solvents and essential oils and high temperature structural pro..