Polymer Property : Oxygen Transmission = 10.0 cc-mm/m²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission 10.0 cc-mm/m²-24hr-atm
25.4 cc-mil/100 in²-24hr-atm
ASTM D3985
Eastman EASTALLOY Polymer DA003-8999K, Clear Alloy  (discontinued **)
Properties below based on a film thickness of 250 microns. CO2 Permeability is 49 cm3·mm/m2·24h·atm per ASTM D 1434.Product Description: EASTALLOY DA003-8999K Polymer is a clear copolyester/pol..
Oxygen Transmission 10.0 cc-mm/m²-24hr-atm
25.4 cc-mil/100 in²-24hr-atm
ASTM D3985
Eastman Eastman 1223 Copolyester
Applications:Blown filmCredit cardsDebit cardsDeodorant packagingElectronic packagingFabricated boxesFlexible packagingFood packagingFurniture/Furniture trimGaming cardsGift cardsIdentification card..
Oxygen Transmission 10.0 cc-mm/m²-24hr-atm
25.4 cc-mil/100 in²-24hr-atm
ASTM D3895
Eastman GSP01 Copolyester for Film and Sheet Extrusion
Applications:Consumer e-packaging trayElectronic packagingElectrostatic dissipative trayProduct Description: GSP01 is a clear, amorphous material. Because of its clarity, toughness and good melt s..