Oxygen Transmission 5.10 cc-mm/m²-24hr-atm
13.0 cc-mil/100 in²-24hr-atm
ASTM D3985
Eastman 9921 PET Film  (discontinued **)
VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p..
Oxygen Transmission 5.10 - 23.0 cc-mm/m²-24hr-atm
13.0 - 58.4 cc-mil/100 in²-24hr-atm
Average value: 11.1 cc-mm/m²-24hr-atm Grade Count:3
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m..
Oxygen Transmission 5.10 cc-mm/m²-24hr-atm
13.0 cc-mil/100 in²-24hr-atm
ASTM D3985
Eastman 9921W PET Film  (discontinued **)
Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters ..