Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 67.0 cc-mm/m²-24hr-atm @Thickness 0.100 mm |
170 cc-mil/100 in²-24hr-atm @Thickness 0.00394 in |
670 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® LED2643 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• LED lighting, optics, .. |