Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 185 - 264 cc-mm/m²-24hr-atm | 470 - 671 cc-mil/100 in²-24hr-atm | Average value: 215 cc-mm/m²-24hr-atm Grade Count:7 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade". Each property range of values reported.. |
|||
Oxygen Transmission | 185 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
470 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
Based on 1 mil (0.0254 mm) thick film; ASTM D3985 |
DuPont Elvax® 3170 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film 18 wt% Vinyl Acetate.Elvax® 3170 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |