Polymer Property : Oxygen Transmission = 2.17 cc-mm/m²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission 2.17 cc-mm/m²-24hr-atm
5.51 cc-mil/100 in²-24hr-atm
Tested per ASTM D3985 at 22°C
DuPont Teijin Films Mylar® OL12 Polyester Packaging Film, 100 Gauge
Data provided by DuPont Packaging Polymers.Mylar® OL12 (formerly known as XM963A) is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat sea..