Polymer Property : Oxygen Transmission = 2.84 cc-mm/m²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission 2.84 cc-mm/m²-24hr-atm
7.21 cc-mil/100 in²-24hr-atm
Tested per ASTM D3985 at 22°C
DuPont Teijin Films Mylar® RL32 Polyester Packaging Film, 75 Gauge
Data provided by DuPont Packaging Polymers.Mylar® RL32 (formerly known as XM999) is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a ..