Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 88.0 cc-mm/m²-24hr-atm | 224 cc-mil/100 in²-24hr-atm | |
Daikin DAI-EL G-501NK Fluoroelastomer Terpolymer, Diamine Curable Grade, 68% Fluorine Content Features: Good mechanical characteristics.Information provided by Daikin Industries. |
|||
Oxygen Transmission | 88.0 - 150 cc-mm/m²-24hr-atm | 224 - 381 cc-mil/100 in²-24hr-atm | Average value: 104 cc-mm/m²-24hr-atm Grade Count:42 |
Overview of materials for Thermoset Fluoroelastomer This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr.. |