Physical Properties Metric English Comments
Oxygen Transmission 229 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
582 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
film; ASTM D3985
DuPont Elvax® 3121A Ethylene-Vinyl Acetate Copolymer Resin for Blown Film  (discontinued **)
7.5 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dr..
Oxygen Transmission 229 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
582 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
film; ASTM D3985
DuPont Elvax® 3165 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
18 wt% Vinyl Acetate.Elvax® 3165 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins..