Oxygen Transmission 1.80 cc-mm/m²-24hr-atm
4.57 cc-mil/100 in²-24hr-atm
or 140 cc/m²-24hr-atm for the film. ASTM D3985
DuPont Teijin Films Mylar® 50 OL Polyester Film, Ovenable Lidding, Heat Sealable, 50 Gauge
Data provided by DuPont Packaging Polymers.An exceptionally strong polyester film designed to package foods. The film is suitable for heating food products in microwave or conventional ovens. Can b..