Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 2.10 cc-mm/m²-24hr-atm | 5.33 cc-mil/100 in²-24hr-atm | or 110 cc/m²-24hr-atm for the film. ASTM D3985 |
DuPont Teijin Films Mylar® 75 OL Polyester Film, 75 Gauge Data provided by DuPont Packaging Polymers.An exceptionally strong polyester film designed to package foods. The film is suitable for heating food products in microwave or conventional ovens. Can b.. |
|||
Oxygen Transmission | 2.10 cc-mm/m²-24hr-atm | 5.33 cc-mil/100 in²-24hr-atm | or 125 cc/m²-24hr-atm for the film. ASTM D3985 |
DuPont Teijin Films Mylar® HS Polyester Film, 65 Gauge (17 µm) Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester packaging film designed for heat shrink applications. It is currently available in 48, 65, 80, and 150 gauges, and othe.. |
|||
Oxygen Transmission | 2.10 cc-mm/m²-24hr-atm | 5.33 cc-mil/100 in²-24hr-atm | or 110 cc/m²-24hr-atm for the film. ASTM D3985 |
DuPont Teijin Films Mylar® LB Polyester Film, 75 Gauge (19 µm) Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester film designed for use as a component of a lamination. Standard thickness offered include 48, 75, and 92 gauges. Variet.. |
|||
Oxygen Transmission | 2.10 cc-mm/m²-24hr-atm | 5.33 cc-mil/100 in²-24hr-atm | or 110 cc/m²-24hr-atm for the film. ASTM D3985 |
DuPont Teijin Films Mylar® LBT Polyester Film, 75 Gauge (19 µm) Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester film that has been corona-treated to provide superior wetting and adhesion to inks, primers, and adhesives. Standard th.. |