Polymer Property : Oxygen Transmission = 511 cc-mil/100 in²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission 201 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
511 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
film; ASTM D3985
DuPont Elvax® 3135X Ethylene-Vinyl Acetate Copolymer Resin for Thin Blown
12 wt% Vinyl Acetate.Elvax® 3135X is an extrudable, ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resi..