Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 23.5 cc-mm/m²-24hr-atm @Temperature 25.0 °C |
59.7 cc-mil/100 in²-24hr-atm @Temperature 77.0 °F |
ASTM D1434 |
Specialty Coating Systems Parylene HT® Poly (P-Xylylene) Coating Parylene HT is a polymer of para-xylylene with the alpha hydrogen atoms of the N dimer replaced with fluorine. This variant of Parylene is useful in high temperature applications (short term up to 4.. |