Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 2.56 cc-mm/m²-24hr-atm | 6.50 cc-mil/100 in²-24hr-atm | Tested per ASTM D3985 at 22°C |
DuPont Teijin Films Mylar® RL33 Polyester Packaging Film, 100 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL33 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film.. |
|||
Oxygen Transmission | 2.56 cc-mm/m²-24hr-atm | 6.50 cc-mil/100 in²-24hr-atm | Tested per ASTM D3985 at 22°C |
DuPont Teijin Films Mylar® RL43 Polyester Packaging Film, 100 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL43 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. Mylar® RL43 is designed to produce stro.. |