Polymer Property : Oxygen Transmission = 64.0 cc-mm/m²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission 64.0 cc-mm/m²-24hr-atm
163 cc-mil/100 in²-24hr-atm
23°C, 50-75% Humidity; ASM D 1434
Advanced Elastomer Systems Trefsin® 3201-65 W305 Thermoplastic Rubber  (discontinued **)
A natural thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing t..
Oxygen Transmission 64.0 cc-mm/m²-24hr-atm
163 cc-mil/100 in²-24hr-atm
23°C, 50-75% Humidity; ASM D 1434
Advanced Elastomer Systems Trefsin® 3101-65 W305 Thermoplastic Rubber  (discontinued **)
A black thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing tec..