Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 2.90 cc-mm/m²-24hr-atm | 7.37 cc-mil/100 in²-24hr-atm | or 75 cc/m²-24hr-atm for the film. ASTM D3985 |
DuPont Teijin Films Mylar® HS Polyester Film, 150 Gauge (38 µm) Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester packaging film designed for heat shrink applications. It is currently available in 48, 65, 80, and 150 gauges, and othe.. |