Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 25.6 - 27.6 cc-mm/m²-24hr-atm | 65.0 - 70.1 cc-mil/100 in²-24hr-atm | ASTM D3985 |
NatureWorks® Ingeo™ 4043D General Purpose Film Grade Biopolymer Ingeo 4043D can be converted into a biaxially oriented film with use temperatures up to 265ºF (130ºC). This film has excellent optics, good machinability and excellent twist and deadfold. These pr.. |
|||
Oxygen Transmission | 25.6 - 27.6 cc-mm/m²-24hr-atm | 65.0 - 70.1 cc-mil/100 in²-24hr-atm | ASTM D3985 |
NatureWorks® Ingeo™ 7001D ISBM Bottle Grade Biopolymer Ingeo biopolymer 7001D is a thermoplastic resin derived from annually renewable resources and is specifically designed for use in injection stretch blow molded (ISBM) bottle applications. Ingeo biop.. |
|||
Oxygen Transmission | 27.6 - 27.6 cc-mm/m²-24hr-atm @Temperature 40.0 - 40.0 °C |
70.1 - 70.1 cc-mil/100 in²-24hr-atm @Temperature 104 - 104 °F |
Average value: 27.6 cc-mm/m²-24hr-atm Grade Count:1 |
Overview of materials for Polychlorotrifluoroethylene; Molded This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu.. |