Polymer Property : Oxygen Transmission = 92.0 cc-mm/m²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission 92.0 cc-mm/m²-24hr-atm
234 cc-mil/100 in²-24hr-atm
or 6100 cc/m²-24hr-atm for the film. ASTM D3985
DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 60 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when exc..