Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Oxygen Transmission = 65.0 cc-mm/m²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission 65.0 cc-mm/m²-24hr-atm

@Thickness 0.100 mm
165 cc-mil/100 in²-24hr-atm

@Thickness 0.00394 in
650 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 1952 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Me..
Oxygen Transmission 65.0 cc-mm/m²-24hr-atm

@Thickness 0.100 mm
165 cc-mil/100 in²-24hr-atm

@Thickness 0.00394 in
650 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 2607 MAS167 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Oxygen Transmission 65.0 cc-mm/m²-24hr-atm

@Thickness 0.100 mm
165 cc-mil/100 in²-24hr-atm

@Thickness 0.00394 in
650 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 2805 MAS145 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Oxygen Transmission 65.0 cc-mm/m²-24hr-atm

@Thickness 0.100 mm
165 cc-mil/100 in²-24hr-atm

@Thickness 0.00394 in
650 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 2805 MAS152 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Oxygen Transmission 65.0 cc-mm/m²-24hr-atm

@Thickness 0.100 mm
165 cc-mil/100 in²-24hr-atm

@Thickness 0.00394 in
650 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 3107 MAS167 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig..
Oxygen Transmission 65.0 cc-mm/m²-24hr-atm

@Thickness 0.100 mm
165 cc-mil/100 in²-24hr-atm

@Thickness 0.00394 in
650 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® ET3127 Polycarbonate
Makrolon® polycarbonate resinMain characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characterist..
Oxygen Transmission 65.0 cc-mm/m²-24hr-atm

@Thickness 0.100 mm
165 cc-mil/100 in²-24hr-atm

@Thickness 0.00394 in
650 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® ET3227 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc..
Copyright © lookpolymers.com All Rights Reserved