Polymer Property : Oxygen Transmission Rate = 48.0 cc/100 in²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission Rate 745 cc/m²/day

@Temperature 23.0 °C
48.0 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
ExxonMobil Bicor™ 30MB666 OPP Film
Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle East, ..
Oxygen Transmission Rate 745 cc/m²/day

@Temperature 23.0 °C
48.0 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
ExxonMobil Bicor™ 30MB668 OPP Film
Product Description: A high speed transparent, biaxially oriented polypropylene film, coated one side very low temperature seal (VLTS) coating. VLTS coating provides excellent performances on high s..
Oxygen Transmission Rate 745 cc/m²/day

@Temperature 23.0 °C
48.0 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
ExxonMobil Bicor™ 30MBR666 OPP Film
Product Description: Bicor 30MBR is a biaxially oriented transparent polypropylene film coated with humidity resistant acrylic on both sides. This film is designed to wrap products with a high moist..
Oxygen Transmission Rate 745 cc/m²/day

@Temperature 23.0 °C
48.0 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
ExxonMobil Bicor™ 32MB600 OPP Film
Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. Gives outstanding performance on overwrap and HFFS machines.Availability: Africa & Middle East, As..
Oxygen Transmission Rate 745 cc/m²/day

@Temperature 23.0 °C
48.0 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
ExxonMobil Oppalyte™ 42MH647 OPP Film
Product Description: A super white opaque, modified higher density, biaxially oriented polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.Ava..
Oxygen Transmission Rate 745 cc/m²/day

@Temperature 23.0 °C
48.0 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
ExxonMobil Oppalyte™ 42MH648 OPP Film
Product Description: A high speed super white opaque, modified higher density, biaxially oriented polypropylene film, acrylic coated one side acrylic, one side very low temperature seal (VLTS) coati..