Polymer Property : Oxygen Transmission Rate = 50.1 cc/m²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission Rate 50.1 cc/m²/day

@Temperature 23.0 °C
3.23 cc/100 in²/day

@Temperature 73.4 °F
Wet, 75% RH; ExxonMobil Method
ExxonMobil Metallyte™ 15MM348 OPP Film
Product Description: An enhanced barrier metalized film with a very broad seal range and can be considered a multipurpose film. This designed of this film allow excellent performance on HFFS machine..
Oxygen Transmission Rate 50.1 cc/m²/day

@Temperature 23.0 °C
3.23 cc/100 in²/day

@Temperature 73.4 °F
Wet, 75% RH; ExxonMobil Method
ExxonMobil Metallyte™ 18MM348 OPP Film
Product Description: An enhanced barrier metalized film with a very broad seal range designed to be used in laminate with OPP or Polyester for HFFS applications. The design of this film allows excel..