Physical Properties Metric English Comments
Environmental Stress Crack Resistance 16 hour
16 hour
F-50; 10% Igepal Cond. B; ASTM D-1693
ExxonMobil Escorene® HD-6704 HDPE, Injection Grade  (discontinued **)
Data Provided by Exxon Chemical Canada.Characteristics: Excellent Toughness, Excellent Stiffness, Excellent ESCRUses: Industrial containers, Industrial lids