Polymer Property : Environmental Stress Crack Resistance = 27 hour Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Environmental Stress Crack Resistance 27 hour
27 hour
FNCT; ISO 16770
Total HDPE 51090 High Density Polyethylene - Blow Molding
HDPE 51090 is a semi high molecular weight (SHMW) high density polyethylene with high resistance to impact and excellent Environmental Stress Crack Resistance. It has been specifically designed for..