Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | 28.0 - 400 hour @Temperature 50.0 - 50.0 °C |
28.0 - 400 hour @Temperature 122 - 122 °F |
Average value: 263 hour Grade Count:5 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade". Each property range of values report.. |
|||
Environmental Stress Crack Resistance | 28.0 - 400 hour @Thickness 2.00 - 2.00 mm |
28.0 - 400 hour @Thickness 0.0787 - 0.0787 in |
Average value: 263 hour Grade Count:5 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade". Each property range of values report.. |