Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | 13.0 - 530 hour @Temperature 40.0 - 50.0 °C |
13.0 - 530 hour @Temperature 104 - 122 °F |
Average value: 240 hour Grade Count:15 |
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum.. |
|||
Environmental Stress Crack Resistance | 13.0 - 530 hour @Thickness 1.90 - 2.00 mm |
13.0 - 530 hour @Thickness 0.0748 - 0.0787 in |
Average value: 240 hour Grade Count:15 |
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum.. |
|||
Environmental Stress Crack Resistance | 530 - 530 hour @Temperature 50.0 - 100 °C |
530 - 530 hour @Temperature 122 - 212 °F |
Average value: 1290 hour Grade Count:8 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |
|||
Environmental Stress Crack Resistance | 530 - 530 hour @Thickness 1.90 - 2.00 mm |
530 - 530 hour @Thickness 0.0748 - 0.0787 in |
Average value: 1290 hour Grade Count:8 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |