Physical Properties | Metric | English | Comments |
---|---|---|---|
Soluble Sulfates | 200 ppm | 200 ppm | |
Old Hickory Volunteer Tennessee Ball Clay A versatile clay selection for casting, pressing, or plastic forming process methods. It is similar to M-23 in mineralogy with slightly more organic content. Volunteer has very good plasticity and i.. |
|||
Soluble Sulfates | 200 ppm | 200 ppm | |
Old Hickory TI-21 Tennessee Ball Clay TI-21 is a very low carbon content clay specifically designed for plastic forming methods. It has excellent oxidation qualities particularly for dense volume stoneware or vitreous ceramic pieces. Th.. |